9:00AM to 7:00PM
The SSS Stainless Steel. & Engg. Co. is a known creator, authority and exporter of Stainless Steel 317/317L Hex Bars, which has higher killjoy, worry to-break and inflexible nature at raised temperature. SS 317 Hex Bars doesn't respond to warm treatment, which can be besides set by contamination working.
Stainless Steel 317L Hex Bars is usually used to oversee sulfur, ruinous dyestuffs, squash alcohol, acetylating and nitrating blends, certifiable coal and oil, obscuring blueprints, and different substance mixes. SS 317 Hex Bars is a higher chromium, nickel and molybdenum modification of SS 316 masterminded fundamentally for expanded quality and breaking down obstruction.
It's fundamental to see that hydrochloric ruinous in any fixation above 5% will rapidly separate austenitic SS 317L Hex Barswith ease. Filler metal or austenitic, low carbon filler metals with molybdenum content higher than that of Alloy 317 Hex Bars, or a nickel-base filler metal with adequate chromium and molybdenum substance to beat the deterioration opposition.
Alloy 317L Hex Bars is the most deterioration safe of the 300 Series composites and has the most basic bendable and creep quality properties at raised temperatures. 317 Stainless Steel Hex Bars will constantly offer better setting/split deterioration check than 304L Stainless Steel, where this is a consequence of the improvement of 2-3% molybdenum. We work by and by with its sellers to guarantee hopeful transparency of 317L Stainless Steel Hex Bars in the structures, sizes, and entireties required by the client.
Dimensions : ASTM, ASME
Standard : ASTM / ASME SA A276, A479, ASTM A493
Length : Random, Fix & Cut Length
Size : 20MM to 150MM
STANDARD | WERKSTOFF NR. | UNS |
SS 317 | 1.4449 | S31700 |
SS 317L | 1.4438 | S31703 |
Element | C | Cr | Mn | Ni | P | S | Si |
SS 317 | 0.08 max. | 18.0 - 20.0 | 2.00 max. | 11.0 - 14.0 | 0.045 max. | 0.03 max. | 1.00 max. |
SS 317L | 0.03 max. | 18.0 - 20.0 | 2.00 max. | 11.0 - 15.0 | 0.045 max. | 0.03 max. | 0.75 max. |
Element | Density | Melting Range,℃ | Tensile Strength | Yield Strength | Elongation | Hardness (Brinell) |
SS 317 | 8 | 1454 ℃ | 515 | 205 | 40 | 217 |
SS 317L | 8 | 1450 ℃ | 515 MPa | 205 | 40 | 217 |