The blend creation of RA330® has changed during an opportunity to consider improved execution in the warm strategy industry. RA330® is the workhorse of the shine safe composites with unimaginable quality and oxidizing hindrance up to 1148°C. Similarly, the amalgam is fantastic in carburising and nitriding conditions.
The properties of RA330® are refreshed by a clear 1.25% silicon augmentation. It has been wanted to withstand warm stun began by fluid splashing. RA330® finds wide applications in high temperature conditions where remarkable security from the joined impact of carburisation and warm cycling conditions are the prime target.
RA330® remains absolutely austenitic at all temperatures so it isn't dependent upon sigma embrittlement. It is remarkably invulnerable to chloride-began pressure deterioration breaking and accordingly a composite of decision where fundamental unadulterated appraisals have assaulted by pressure use separating.
RA330® can be made and machined utilizing approach utilized for treated steels or nickel-chromium mixes. Warmth treatment isn't fundamental after generally circling and welding endeavors. Right when required, the supported full toughen is 1038-1371°C, energetic air cool or water drench. RA330® can be in a split second welded utilizing RA330-04® or other weld fillers of arranging conditions.
Product form | Size range from | Size range to |
---|---|---|
RA330® expanded metal | To customer specifications | To customer specifications |
RA330® pipe | 0.5 in | 152.4 in |
RA330® round bar | 3.175 mm | 152.4 mm |
RA330® sheet & plate | 1.22 mm | 76.2 mm |
RA330® welding wire | 0.89 mm | 3.175 mm |
RA330® coil | 3 mm | 4 mm |
RA330® pipe fittings | 3 mm | 4 mm |
% | Cr | Ni | Si | C | Mn | P | S | Cu | Fe |
---|---|---|---|---|---|---|---|---|---|
Min | 18 | 34 | 1 | - | - | - | - | - | Balance |
Max | 20 | 37 | 1.50 | 0.08 | 2 | 0.03 | 0.03 | 1 | - |
Mechanical & Physical Properties | 21°C | 538°C | 593°C | 649°C | 704°C | 760°C | 816°C | 871°C | 982°C | 1093°C |
---|---|---|---|---|---|---|---|---|---|---|
Ultimate Tensile Strength /MPa | 586.1 | 489.5 | 457.8 | 390.9 | 305.4 | 247.5 | 184.8 | 145.5 | 71.7 | 22.1 |
0.2% Yield Strength /MPa | 268.9 | 172.4 | 166.9 | 151.7 | 144.8 | 142.7 | 119.3 | 106.2 | 58.6 | 13.8 |
Elongation | 47 | 46 | 46 | 43 | 69 | 78 | 56 | 79 | 79 | 28 |
Minimum Creep 0.0001% per hr /MPa | - | - | - | - | - | 24.8 | - | 14.5 | 3.4 | - |
10,000 hr Rupture Strength/MPa | - | - | - | - | 29.6 | - | 11.7 | 4.3 | 1.9 | |
Coefficient of Thermal Expansion /µm/m⁰C | - | - | - | - | - | 17.46 | - | 17.64 | 18 | - |
Thermal Conductivity /kcal/(hr.m.°C) | 10.71 | - | - | - | - | 20.39 | - | 21.13 | 21.87 | - |
Modulus of Elasticity / x105 MPa | 2 | - | - | - | - | 1 | - | 1 | 1 | - |